No. 539 Stress Cracking Instruments

Description

The Stress Cracking Instruments are jiggers for handling samples which always enables to perform correct and definite bending stress cracking test under a constant condition.

Specifications

Specimen size 38 x 12.7mm
Notch depth Method A: 0.5 to 0.65mm 

Method B & C: 0.3 to 0.4mm

Dimensions Slitter: W70 x H30 x L280mm 

Bending clamp: W30 x H60 x L170mm

Transfer tool: W80 x H20 x L390mm

Mass (Approx.) Slitter: 2kg 

Bending clamp: 1.5kg

Transfer tool: 2kg

Related standards

ASTM D1693