Our Products

De Mattia Flex-Cracking Tester | No.255/263

Description

The De Mattia Flex-Cracking Tester measures endurance of rubber specimens with regard to repeated bending and length of crack generated due to repeated bending.

Specifications

Catalog No. 255 263
Model DM-01 G7A-L
Number of specimens 12 specimens max. 20 specimens max.
Flex speed 300±10 times/min.
Flex stroke 57mm fixed 0 to 100mm
Flex counter 6 digits counter 8 digits counter
Temperature range RT(+40°C) to 150°C
Break detection Laser type break detection device
Power supply Single-phase, AC100V, 50/60Hz, 0.7kVA

(230V, 115V etc. using step-down transformer)

Three-phase, AC200V, 50/60Hz, 5.9kVA

(415V, 380V etc. using step-down transformer)

Dimensions W450 × D450 × H600 mm W1270 × D1050 × H1500mm
Weight (Approx.) 78kg 700kg

Related standards

ISO 132 Rubber, vulcanized or thermoplastic — Determination of flex cracking and crack growth (De Mattia)
ASTM D813 Standard Test Method for Rubber Deterioration—Crack Growth